http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016000462-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9caeda0ed267f6d24b739b5b1eb2ad48 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L33-60 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B15-08 |
filingDate | 2014-06-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_db3fdc697522ea89886e7b9dadb9c5c4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_27804c2991b91fa5e2a1f01633f2db8e |
publicationDate | 2016-01-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2016000462-A |
titleOfInvention | Substrate |
abstract | An object of the present invention is to provide a substrate exhibiting good whiteness even in a high temperature environment. A substrate according to the present invention includes at least a resin layer. The resin layer contains a resin mainly composed of a polyimide resin. And this base | substrate has the Hunter whiteness of the resin layer after heat-processing for 60 minutes at 260 degreeC being 84% or more. This substrate preferably has a hunter whiteness maintenance rate of 93% or more after heat treatment at 260 ° C. for 60 minutes, and the total light reflection on the resin layer side after heat treatment at 260 ° C. for 60 minutes. The rate is preferably 75% or more, and the maintenance ratio of the total light reflectance on the resin layer side after heat treatment at 260 ° C. for 60 minutes is preferably 94% or more. [Selection] Figure 2 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7189619-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2018186215-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2018186215-A1 |