http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015217546-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f4d9d138d23c7ca8bfae3daf28b4eba0 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-36 |
filingDate | 2014-05-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5389744ad647afa68c10ba2b3b932c7c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a9bc54453ba3b91ba1d3c82e83fb89f0 |
publicationDate | 2015-12-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2015217546-A |
titleOfInvention | Phase difference film manufacturing process Polyester film for paper base |
abstract | PROBLEM TO BE SOLVED: To suppress the amount of oligomer precipitation in a hard coat film used in a retardation film production process, improve the reusability of the hard coat film, and in the retardation film without deforming the hard coat film, Retardation film manufacturing process paper hard coat that can obtain high-quality and stable retardation film with a thin thickness band, which is the required quality in recent years, without the occurrence of defects such as unevenness and excellent flatness A polyester film for a film substrate is provided. SOLUTION: A hard coat layer is provided on one surface, the surface roughness (Ra) of the other surface is 70 to 120 nm, and the intrinsic viscosity of the polyester layer constituting the surface is 0.67 or more. A polyester film having a total thickness of 70 to 155 μm. [Selection figure] None |
priorityDate | 2014-05-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |