http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015196808-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_33dafb5bbc2ec47ebcb7becbbe60f704 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-13 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L29-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-20 |
filingDate | 2014-04-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1402bd868ec331bf72b13f967f883302 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c1c9c39f8583c75dda5cfd362f6722b0 |
publicationDate | 2015-11-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2015196808-A |
titleOfInvention | Production method of polyvinyl alcohol film |
abstract | [Problem] To provide a method for producing a PVA film capable of easily producing a polyvinyl alcohol film having a small color and a smooth surface, and a polyvinyl alcohol film produced thereby. A method for producing a polyvinyl alcohol film containing a surfactant and an antioxidant, the method comprising a step of mixing a mixture of a surfactant and an antioxidant and polyvinyl alcohol, and thereby A manufactured polyvinyl alcohol film. In the mixture of the surfactant and the antioxidant, the antioxidant is preferably dispersed in the surfactant. Moreover, it is preferable that the usage-amount of antioxidant is 1-9 ppm on a mass basis with respect to polyvinyl alcohol. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111954695-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2021171882-A1 |
priorityDate | 2014-04-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 58.