http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015196262-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_962adbf7d50e742218f3d536a63df612 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-00 |
filingDate | 2014-03-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_326784880477f20f132daf2b8a9891c7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ea7f82e942b194ef5ffd786c81a9b5b7 |
publicationDate | 2015-11-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2015196262-A |
titleOfInvention | Release film and adhesive |
abstract | PROBLEM TO BE SOLVED: To provide a release film capable of suppressing or preventing the formation of a plurality of minute irregularities (skin skin) on an adhesive surface of an adhesive layer provided on the surface of a release agent layer. Providing and providing a pressure-sensitive adhesive body provided with such a release film. A release film of the present invention is a release film that is detachably attached to an adhesive layer, and includes a base material 11 and a release agent layer 12 provided on one surface 111 side of the base material 11. The surface free energy γ total of the release agent layer 12 satisfies the relationship of 11 [mJ / m 2 ] <γ total <15 [mJ / m 2 ], and the dispersion of the surface free energy γ total The component γ d satisfies the relationship of 8 [mJ / m 2 ] <γ d <11 [mJ / m 2 ]. [Selection] Figure 1 |