assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_74415d2d575191b74012a38dc7a41110 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B14-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B20-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-02 |
filingDate | 2014-03-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a29124aa9ef49be2120b8031611df9e8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f017365c1134a59dac7c200b6ea2f2b5 |
publicationDate | 2015-11-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2015189613-A |
titleOfInvention | Concrete composition and method for producing concrete composition |
abstract | A concrete composition having a high compressive strength with reduced drying shrinkage strain and a method for producing the concrete composition are provided. A concrete composition containing fine aggregate containing hard sandstone, coarse aggregate, cement, and water, wherein the weight average grain of the hard sandstone contained in the entire fine aggregate in the concrete composition A concrete composition characterized by having a diameter D50 exceeding 0.85 mm, and a method for producing a concrete composition comprising kneading fine aggregate containing hard sandstone, coarse aggregate, cement, and water. The manufacturing method of the concrete composition which adjusts the particle size of this hard sandstone so that the weight average particle diameter D50 of the hard sandstone contained in the whole fine aggregate may exceed 0.85 mm. [Selection figure] None |
priorityDate | 2014-03-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |