http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015187715-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_758994071efb42b565fc2c04637be131 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-09 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-087 |
filingDate | 2015-03-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9e10ea5a2bcad7f66c150fce218b433f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0637aef106f4f68b697b39c5590d0db0 |
publicationDate | 2015-10-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2015187715-A |
titleOfInvention | Toner manufacturing method and toner |
abstract | The present invention provides a method for producing a toner which can achieve both heat-resistant storage stability, moisture-heat storage resistance and low-temperature fixability, and has excellent toner durability and gloss. A method for producing a toner (Z) comprising a colorant, a crystalline resin (A), and a vinyl resin (B) having an ester group, wherein the colorant, the crystalline resin (A) and vinyl are first produced. Toner (Z) including a step of heating and fusing the aggregate (Y) obtained by aggregating the dispersion (X) in the dispersion (W) containing the resin (B) to obtain resin particles (Z ′). ) Manufacturing method. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019015977-A |
priorityDate | 2014-03-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 809.