http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015186912-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7f9af914ed2fb00cd4f1b8b1a28964e4 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C55-02 |
filingDate | 2015-01-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_61a1d4da10ae3a4cfd5510db9cd65c1b |
publicationDate | 2015-10-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2015186912-A |
titleOfInvention | Manufacturing method of optical film |
abstract | 【Task】 Provided is a method for producing an optical film that reduces quality defects such as creases caused by wrinkles inside an optical film roll that occurs during winding or over time when a stretched optical film is produced, and has high productivity. [Solution] In a method for producing an optical film, which is molded using a thermoplastic resin containing a specific acrylic polymer and obtained through a stretching process and a winding process, the film is wound at a speed of 10 m / min to 200 m / min while pressing the optical film. It has been found that the above-mentioned problems can be solved by using a winder having a touch roll that can be wound at a speed and performing a winding process in which the temperature of the touch roll is adjusted to 3 ° C. or higher and 15 ° C. or lower. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2022107491-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2022082376-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7097939-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-I798880-B |
priorityDate | 2014-03-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 58.