http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015152823-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e643df164d408263905077a4d3016558 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G15-0818 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G15-0808 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L9-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L9-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G15-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F16C13-00 |
filingDate | 2014-02-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e3d86176bdfd724c7e190576528b83e5 |
publicationDate | 2015-08-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2015152823-A |
titleOfInvention | Semi-conductive roller |
abstract | In particular, when combined with a positively charged non-magnetic one-component toner, a high toner charge amount can be imparted to the toner, and it can also function as a developing roller having excellent toner retention by mirror image force. Provide a roller. A semiconductive roller 1 is formed by a cross-linked product containing only two kinds of butadiene rubber and epichlorohydrin rubber as rubber components. The blending ratio of butadiene rubber is preferably 20 parts by mass or more and 90 parts by mass or less in 100 parts by mass of the total amount of rubber. [Selection] Figure 1 |