http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015151491-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_32ce12f8709350afe097badddf523729 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L71-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-3477 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-00 |
filingDate | 2014-02-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8767e0814c03a292984fbfc496c9492a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_af57bc93f57067442ac5cb28f77767b6 |
publicationDate | 2015-08-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2015151491-A |
titleOfInvention | Laminate containing PPE |
abstract | The present invention provides a laminate and a method for producing the same, which prevents deterioration of electrical characteristics over time and maintains good electrical characteristics inherent in PPE. A laminate comprising polyphenylene ether (A) and an organic solvent (B), wherein the organic solvent (B) has the following boiling points at (a) to (c): (a) 1 atm. Is 120 ° C. or higher, (b) the octanol / water partition coefficient Log POW is 0.04 or more and 4.00 or less, and (c) the amount contained in the laminate is 0.01 A laminated board satisfying that the content is 1% by mass or more. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2018061736-A1 |
priorityDate | 2014-02-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 20.