abstract |
To provide a resin composition capable of obtaining a molded article having excellent scratch resistance and mechanical properties, low gloss, and low shrinkage anisotropy. A propylene polymerized material (A) containing 50 wt% or more of a structural unit derived from propylene (A) 40 wt% or more and 90 wt% or less, and wollastonite (B) is 9 wt% or more and 30 wt% or less, Elastomer (C) is a resin composition containing 1 wt% or more and 30 wt% or less (provided that the total amount of (A), (B) and (C) is 100 wt%), A resin composition in which wollastonite (B) satisfies specific requirements. [Selection figure] None |