http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015089980-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1374dd16777534b65ad4422333245af8 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-04 |
filingDate | 2013-11-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b96c6d4064bcb0deed14c8dc0290d490 |
publicationDate | 2015-05-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2015089980-A |
titleOfInvention | Polyethylene fiber |
abstract | Disclosed is a polyethylene fiber that can be suitably used for apparel applications that are excellent in coolness and easy to handle and process. A fiber comprising polyethylene as a main component, wherein the polyethylene has an intrinsic viscosity of 0.8 to 1.7, a breaking strength of 2 to 8 cN / dtex, and a boiling water shrinkage of 2 to 5%. Polyethylene fiber characterized by being. Furthermore, the fiber cross-sectional shape is preferably flat. Another method for producing a polyethylene fiber according to the present invention is to melt-spin, stretch, and heat-set a resin mainly composed of polyethylene having an intrinsic viscosity of 0.8 to 1.7 and contact a heat medium. Is a manufacturing method characterized by [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102167737-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2021132768-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102183247-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20200036171-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113710836-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-114502784-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-114502784-B |
priorityDate | 2013-11-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 21.