Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7f9af914ed2fb00cd4f1b8b1a28964e4 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L79-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-56 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-54 |
filingDate |
2013-11-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_be51ebbc383c63a342a62df2d555299f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6fe51c0581c2001b827b66682c9d0b93 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d7746daf79d242611e022246c9b543c2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fc7763c772b8b0eee8396e0cf5ef4f4b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_10cccbb6d1127ee7b139ecd77515b186 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_19834520e335fe7396702e2626eaed64 |
publicationDate |
2015-05-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2015089899-A |
titleOfInvention |
Thermosetting resin composition |
abstract |
PROBLEM TO BE SOLVED: To reduce the mechanical strength of a cured product comprising a cyanate ester compound, which can be cured at a curing temperature of 200 ° C. or less and exposed to high temperature air exceeding 200 ° C. for a long time. A thermosetting resin composition that can be suppressed is provided. A thermosetting resin composition comprising a cyanate ester compound and a metallocene compound. [Selection figure] None |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017023966-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-110343246-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2019124558-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20200055799-A |
priorityDate |
2013-11-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |