http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015083672-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9e1bf06f55de84b78abc9a057807f7eb |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C45-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-04 |
filingDate | 2014-09-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3127740f231ba5929089bca2347288e6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5a4ee92ac8b98ade650456ecafa7e54c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_83ce340eac19c637dfd469d6e4c33ecc http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_16ccd027a139cf61b7597d4e88d91a5d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c9cbf974a36382ec5b9a5d7d3915cd49 |
publicationDate | 2015-04-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2015083672-A |
titleOfInvention | Polylactic acid resin composition for injection foaming, injection foam molded article, and method for producing injection foam molded article |
abstract | A polylactic acid resin composition capable of efficiently obtaining an injection foam molded article having excellent heat resistance and good strength, and an injection foam molded article using the resin composition. A resin composition comprising 0.1 to 10 parts by mass of a crystal nucleating agent (B) with respect to 100 parts by mass of a polylactic acid resin (A), the following (1) to (3) A polylactic acid resin composition for injection foaming that satisfies the above conditions simultaneously. (1) Crystallization rate index is 0.3 to 20 (min) (2) The D-form content of the polylactic acid resin (A) is 2.0 mol% or less, or 98.0 mol or more (3) 190 ° C. For injection foaming in which the melt viscosity measured under 21.6N condition is 0.1 to 30 g / 10 min, and the foaming agent (C) is contained in an amount of 0.01 to 2 parts by mass with respect to 100 parts by mass of the composition. Polylactic acid resin composition [selection figure] None |