http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015081305-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_20d3042eb4ea7c9afd525aa89373349d |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-66 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-42 |
filingDate | 2013-10-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_978c9fd1ee4359ee78b6d8cdf1e3488a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4bfdfc925bc78f8db957af872cc343fc |
publicationDate | 2015-04-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2015081305-A |
titleOfInvention | Polyurethane elastomer and elastic fiber |
abstract | PROBLEM TO BE SOLVED: To provide an excellent support feeling by exhibiting an unprecedented elastic recovery behavior in which the return after elongation is moderately slow immediately after wearing and gradually recovers elastically but the final strain is small. An elastomer and an elastic fiber using the same are provided. A polyurethane elastomer obtained by reacting a polyester polyol (A) having an aromatic skeleton, a diol (B) having an aliphatic skeleton having 2 to 6 carbon atoms, and a diisocyanate (C), [Condition 1] The tan δ peak temperature of a film having a thickness of 50 μm is 0 to 40 ° C., and [Condition 2] the instantaneous strain (α) of the film is 150 to 200% and the permanent strain (β) is 10% or less. Both of these conditions are satisfied. [Selection] Figure 1 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11286328-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018536059-A |
priorityDate | 2013-10-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 70.