http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015081260-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_cebc9740ef706cde29e885504f274ffa |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L55-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-06 |
filingDate | 2013-10-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4b4c1c1498dcc6b5e1c38bf1e2e76b19 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5ef34297e7f71c21c739f99df2c03341 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_acd724eb94a1be748faf2a67ad25f83e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ade0ec40fb74bba01951a9cb2929f5ac |
publicationDate | 2015-04-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2015081260-A |
titleOfInvention | Resin composition and film |
abstract | PROBLEM TO BE SOLVED: To provide a resin composition containing an acrylic resin with improved thermal properties and mechanical properties and a film thereof. A resin composition comprising an acrylic copolymer (A) having a weight average molecular weight of 40,000 or more and less than 200,000 and an acrylic copolymer (B) having a weight average molecular weight of 200,000 or more, wherein the acrylic A copolymer obtained by polymerizing a monomer mixture (M) in which the copolymer (A) has a glass transition temperature of 115 ° C. or more and 135 ° C. or less and the acrylic copolymer (B) contains a macromonomer. A resin composition. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2017077951-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2017077908-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017206606-A |
priorityDate | 2013-10-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 143.