Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_cd23c354dd49d149991d5e4d2af08b17 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L1-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-105 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-06 |
filingDate |
2014-11-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_46432adf4086eba5f069e0736683b9eb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_aa839f5f52b4ca74c9996e289f25fb85 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e75a1e8b21a2b11c4749f3a667ecfaab http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3e111efcc5c82499d53b59ac13baad31 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b48542f4fdb60570f0da7e7451987f9b |
publicationDate |
2015-04-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2015071770-A |
titleOfInvention |
Cellulosic resin composition |
abstract |
The present invention provides a plasticizer capable of plasticizing cellulose ester in a melt-kneading system. SOLUTION: 100 parts by weight of a cellulose ester such as cellulose triacetate is melt-kneaded with 0.5 to 50 parts by weight of a fluorene compound having a 9,9-bisarylfluorene skeleton represented by the formula (1). How to plasticize. (Ring A is a benzene ring or naphthalene ring; X1 is a hydroxyl group; R1 is a C2-4 alkylene group; k is 0 to 2; m is 1 or 2; R2 is a methyl group or a phenyl group; n is 0 or 1) Selection diagram] None |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019535869-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-6326157-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7208135-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018131506-A |
priorityDate |
2014-11-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |