http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015031915-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7f9af914ed2fb00cd4f1b8b1a28964e4 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-08 |
filingDate | 2013-08-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_71d471c6ab13d4f8bbdd27e4e2e10dbd http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_aaf5d31085a407147c88b3f54bde30b7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f8c522358d8ebd336a617b9453bbad0c |
publicationDate | 2015-02-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2015031915-A |
titleOfInvention | Toner additive and toner for developing electrostatic image |
abstract | To provide a positively chargeable toner additive capable of improving the negative chargeability of a negatively chargeable toner. An additive for toner of the present invention includes resin particles having at least a surface layer formed of an amino-based resin and a hydrophobic inorganic oxide, and the content ratio of the hydrophobic inorganic oxide is the resin particles. It is 0.05 to 10 parts by weight with respect to 100 parts by weight, the average particle diameter of the resin particles is 780 nm or less, and the average particle diameter of the hydrophobic inorganic oxide is 80 nm or less, The hydrophobicity of the hydrophobic inorganic oxide is 45% or more. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019056744-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017037258-A |
priorityDate | 2013-08-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 69.