http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015016509-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8fb9f44db08d1c42a53f3d28eaae416f |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-07 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-053 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22C1-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22C1-10 |
filingDate | 2014-10-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a31de95e9f0e731579ae4b39b855377c |
publicationDate | 2015-01-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2015016509-A |
titleOfInvention | Self-hardening mold composition |
abstract | The present invention provides a self-hardening mold composition, a binder composition, and a mold production method using the same, which can improve the deep curability of the mold. A self-hardening mold composition obtained by mixing a refractory particle, a binder composition containing an acid curable resin, and a curing agent, represented by the following general formula (1): At least one compound (A) selected from the group consisting of dihydric alcohols, ether group-containing dihydric alcohols represented by the following general formula (2) and ketones represented by the following general formula (3): A self-hardening mold composition containing 0.0049 to 0.069% by weight in the self-hardening mold composition. HO-R1-OH (1) HO- (R2O) n-H (2) R3-CO-R4 (3) [Selection] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017030009-A |
priorityDate | 2014-10-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 112.