http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014500386-A
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L69-00 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-5317 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L67-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-199 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-85 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-5317 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-199 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-02 |
filingDate | 2011-12-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2014-01-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2014500386-A |
titleOfInvention | Color improvement in titanium catalyzed polyester. |
abstract | In one embodiment of the present invention, (a) (i) 70-100 mol% terephthalic acid residue, (ii) 0-30 mol% aromatic dicarboxylic acid residue having 20 or fewer carbon atoms, and (iii) ) An aliphatic dicarboxylic acid residue having no more than 16 carbon atoms, a dicarboxylic acid component comprising 0-10 mol%, and (b) the following (i) and (ii): (i) an ethylene glycol residue And (ii) a cyclohexanedimethanol residue, a glycol component comprising about 90 to about 10 mol%, and (II) a residue of at least one titanium compound, and (III) structure (II) : Wherein n is an integer from 1 to 4, R can be hydrogen or C 1 -C 22 alkyl, and R 1 and R 2 are each hydrogen, C 1 -C 22 alkyl, hydroxyl Or it can be aryl. A polyester containing at least one chelating phosphorus species, a reaction product thereof, or a mixture thereof, wherein the total mol% of the dicarboxylic acid component is 100 mol%, and the total of the glycol components The intrinsic viscosity of the polyester was measured in 60/40 (wt / wt) phenol / tetrachloroethane at a concentration of 0.25 g / 50 ml at a temperature of 25 ° C. The polyester is 0.35 to 1.2 dL / g. |
priorityDate | 2010-12-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links