http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014205796-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6c8d4dc7bd1a30d8fda907fceaeb4e69 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-183 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-78 |
filingDate | 2013-04-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b98b1b922ae0098ccaac331dd51c6cf9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6e106124a0efcd5910c5661aca2fb022 |
publicationDate | 2014-10-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2014205796-A |
titleOfInvention | Polyester resin and method for producing the same |
abstract | An object of the present invention is to provide a polyester resin suitable for reducing haze of a molded product while shortening a filling time in injection molding and a method for producing the same. A polyester resin produced from a dicarboxylic acid component having terephthalic acid or an ester-forming derivative thereof as a main component and a diol component having ethylene glycol as a main component, and having an acetaldehyde content of 10 ppm by weight or less. Polyester resin in which the intrinsic viscosity IV satisfies the following formula (1), and the haze of a 5 mm-thick molded plate injection molded at a cylinder temperature of 280 ° C. and a mold temperature of 21 ° C. is 3% or less. Intrinsic viscosity 0.68 IV IV 0.7 0.77 dL / g (1) [Selection] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-115335430-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-115335430-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2021192962-A1 |
priorityDate | 2013-04-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |