http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014173004-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e643df164d408263905077a4d3016558 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K3-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F16J15-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F265-00 |
filingDate | 2013-03-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4aec4f81514cec2c528154ea221aa530 |
publicationDate | 2014-09-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2014173004-A |
titleOfInvention | Surface modification method for three-dimensional object and gasket for syringe |
abstract | A method for modifying a surface of a three-dimensional object, which can simultaneously improve the surface of a plurality of three-dimensional objects, and impart performance such as good slidability, durability against repeated sliding and sealing properties, and the like A syringe gasket obtained by the surface modification method is provided. SOLUTION: A step 1 of immersing a plurality of three-dimensionally shaped products in a photopolymerizable monomer-containing liquid, and while stirring the photopolymerizable monomer-containing liquid, the photopolymerizable monomer is polymerized by light irradiation, and the plural And a step 2 of growing a polymer chain on the surface of the three-dimensional object. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2018198876-A1 |
priorityDate | 2013-03-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 112.