http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014123059-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d93502a23a72b56472bc75854cfe7c60 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02F1-13363 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02F1-1335 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-30 |
filingDate | 2012-12-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_376ee8d15ecdd772c20ddff75b26d4c7 |
publicationDate | 2014-07-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2014123059-A |
titleOfInvention | Retardation film laminate and method for producing the same, polarizing plate laminate, and liquid crystal display device |
abstract | A retardation film laminate that hardly causes curling is provided. A layer composed of a first resin (A) containing a polymer having an alicyclic structure; a B layer composed of a second resin (B) containing a polymer having an alicyclic structure; A C layer made of a thermoplastic resin (C) and peelable from the B layer in this order, the glass transition temperature of the first resin (A) is TgA, and the glass transition of the second resin (B) A retardation film laminate satisfying TgA + 10 ° C. ≦ TgB and TgA−10 ° C. ≦ TgC ≦ TgA + 10 ° C. when the temperature is TgB and the glass transition temperature of the thermoplastic resin (C) is TgC. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016118698-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016122176-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019086792-A |
priorityDate | 2012-12-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 98.