http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014118460-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b55c349b43c3ecba4977fd52cc8f8c67 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J201-00 |
filingDate | 2012-12-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bb63212b56ff24ba8b5ada27d6a2bd3c |
publicationDate | 2014-06-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2014118460-A |
titleOfInvention | Temperature-responsive sheet and temperature-responsive adhesive tape |
abstract | PROBLEM TO BE SOLVED: To provide a temperature-responsive sheet in which the adhesive strength becomes higher than the initial adhesive strength when exposed to high temperature, and the normal-temperature adhesive strength does not increase excessively even when exposed to a high temperature for a long time. To do. A peel adhesive strength at a temperature of 25 ° C. is 0.1 N / 10 mm or less, and a peel adhesive strength at any temperature within a range of 120 to 200 ° C. is 0.1 N / 10 mm or more, A temperature-responsive sheet having a peel adhesive strength to the polyethylene naphthalate film of 0.5 N / 10 mm or less after being attached to a polyethylene naphthalate film, heated at 150 ° C. for 2 hours, and then allowed to stand at 25 ° C. for 3 hours. . [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-110431205-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-110431205-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2018181453-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-114921084-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016092308-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020139159-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018009105-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7104742-B2 |
priorityDate | 2012-12-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |