http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014117940-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6bfdf49224a405be1f7b653c56ebad94 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B1-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-32 |
filingDate | 2012-12-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b935795f4d12cfcacf3f41c17ef4fe29 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_86020d7c9b18ac9698674c35eb1d06d0 |
publicationDate | 2014-06-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2014117940-A |
titleOfInvention | Multi-layer hollow container |
abstract | PROBLEM TO BE SOLVED: To provide a multilayer container excellent in aroma retention, cleanliness, heat resistance and transparency. An inner layer made of low density polyethylene (1) having a melt flow rate of 0.1 g / 10 min to 20 g / 10 min, a density of 890 kg / m 3 to 940 kg / m 3 , and a melt flow rate of 0 .1 g / 10 min or more and 10 g / 10 min or less, melt tension at 160 ° C. of 20 mN or more, strain hardening property, density of 920 kg / m 3 or more and 955 kg / m 3 or less, melting point measured by DSC of 1 An intermediate layer comprising an ethylene / α-olefin copolymer (2) having a melt flow rate of 0.1 g / 10 min to 20 g / 10 min and a density of 890 kg / m 3 to 940 kg / m 3 Multi-layer hollow container consisting of an outer layer made of low-density polyethylene (3) [Selection] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015199829-A |
priorityDate | 2012-12-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |