http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014114439-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_758994071efb42b565fc2c04637be131 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K3-16 |
filingDate | 2013-11-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cf0250ea1764f38d6a863bf38b2cda1b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c860e23b4c172896f82d79601ab8ef49 |
publicationDate | 2014-06-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2014114439-A |
titleOfInvention | Antistatic agent and antistatic resin composition containing the same |
abstract | An antistatic agent capable of imparting sufficient permanent antistatic properties to a molded article even when added in a small amount without impairing the appearance and mechanical strength of the molded article, and an antistatic resin composition containing the same. The purpose is to provide. In a 1,3-dioxo-2-oxapropylene group of a copolymer (A) obtained by copolymerizing an unsaturated aliphatic hydrocarbon (a) and an unsaturated acid anhydride (b), An antistatic agent comprising a compound (C) obtained by esterifying a valent hydroxyl group-containing compound (B) and an onium salt (D), wherein the molar ratio of (a) to (b) in the copolymer (A) The antistatic agent whose {(a) / (b)} is 95/5 to 25/75 and (B) is a hydroxyl group-containing compound having a polyethylene oxide chain with a degree of polymerization of 10 to 100. [Selection figure] None |