http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014091854-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9c12ab86c9344c1de6e324177995c149 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G11B7-24035 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C14-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G11B7-243 |
filingDate | 2012-11-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1531db3aaeea83a7b185f549623e51d1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3c4a465b2ed9bf7aa56361c33af101fb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_aa5f66b289168901d958660c7d2a179b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9b819312849591463ab8b75ff35a8815 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_807d93695c0e13d964db386e1bdd4df8 |
publicationDate | 2014-05-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2014091854-A |
titleOfInvention | Alloy target for recording layer, recording layer, optical recording medium, and Blu-ray disc including the same |
abstract | The present invention provides an alloy target including a (Cu a Si b ) X M 1-X alloy, a recording layer, an optical recording medium, and a Blu-ray disc including the same. [Solution] The present invention provides an alloy target including a (Cu a Si b ) X M 1-X alloy, a recording layer, an optical recording medium, and a Blu-ray disc including the same, so that the phase change temperature of the conventional dual recording layer is increased. It solves problems such as the burning speed of the optical recording medium being limited due to being too high, and the recording quality being deteriorated. The anti-corrosive element (M) described above can prevent the oxidation of copper metal from occurring. Further, by setting the phase change temperature of the (Cu a Si b ) X M 1-X alloy from 150 ° C. to 425 ° C., an alloy material suitable for the recording layer of the optical recording medium is obtained. Therefore, the present invention includes that the Blu-ray disc of (Cu a Si b ) X M 1-X alloy has the advantages of being highly stable and capable of high-speed burning at the same time. [Selection] Figure 4 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-108281159-A |
priorityDate | 2012-11-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |