http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014080486-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_06ea9f956e87fb918ac61ef4acb5b2be |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F291-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-04 |
filingDate | 2012-10-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f09c6e76b8b6cd06a21cbddead975159 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2d19ce09097033d2d1b950caf9104605 |
publicationDate | 2014-05-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2014080486-A |
titleOfInvention | Rubber-modified thermoplastic elastomer |
abstract | Provided are a rubber-modified thermoplastic elastomer having low tackiness and high softness, and a rubber-modified thermoplastic elastomer composition containing the rubber-modified thermoplastic elastomer and other thermoplastic resins. An aromatic vinyl monomer and another monomer copolymerizable with an aromatic vinyl monomer in the presence of 70 to 95 parts by weight of a rubbery polymer (a) A rubber-modified thermoplastic elastomer obtained by emulsion polymerization of a part, having a graft ratio of 4 to 35% and a storage elastic modulus of acetone insoluble content measured under the following conditions of 0.5 to 40 MPa . [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016175971-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017031362-A |
priorityDate | 2012-10-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 113.