http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014074086-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_dc45703f67bc72a6db582867886fd5d5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_915269922949d81a90260e5cd5d2df40 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-50 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M8-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M8-10 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B1-06 |
filingDate | 2012-10-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0fe61b25d441085c5c8554f2feeb8cc8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7b82a658ec96ce0d3dade7690c612d3a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7dccc912d5d1a32241e40f3d38149158 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d5e46dbd4e1248d548c7cf7251e7ae27 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b21837c549f3847dd663e82fc5150ef1 |
publicationDate | 2014-04-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2014074086-A |
titleOfInvention | Organic-organic composite solid electrolyte and electrolyte membrane |
abstract | An organic-organic composite solid electrolyte that can improve the hydrogen peroxide resistance of hydrocarbon-based electrolytes and perfluoro-based electrolytes and that is less likely to reduce battery performance, and an electrolyte membrane using the same To do. In an organic solvent having a dielectric constant of 10 or less, an additive composed of an organic compound containing neither S nor a metal element and containing N and / or O is dissolved. An additive solution is prepared, the additive solution and the solid polymer electrolyte are brought into contact, and then the low dielectric constant organic solvent is volatilized from the solid polymer electrolyte. In this case, before contact with the additive solution or after contact with the additive solution, and after volatilizing the low dielectric constant organic solvent, the solid polymer electrolyte and water or pH are 3 You may make it contact with the aqueous solution below 9 or more. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016221425-A |
priorityDate | 2012-10-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 743.