http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014043504-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9e1bf06f55de84b78abc9a057807f7eb |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-04 |
filingDate | 2012-08-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_73b9afa60891df40861bb12d9f37f3f7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_64d490128209525f4c1d5660dc07a4de |
publicationDate | 2014-03-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2014043504-A |
titleOfInvention | Resin composition |
abstract | A resin composition comprising a polylactic acid resin and an acrylic resin, having sufficient transparency and heat resistance, and having sufficient flexibility and impact resistance against falling ball impact and falling weight impact. Offer things. A polylactic acid resin (A), a polymethyl methacrylate resin (B), and a methyl methacrylate / n-butyl acrylate copolymer (C) are contained, and (A) and (B) The mass ratio ((A) / (B)) is 28/72 to 35/65, and the total content of (A) and (B) is 100 parts by mass, and the content of (C) is 9 to It is 14 parts by mass, the deflection temperature under load at 1.8 MPa of (B) is 95 ° C. or more, and the content of n-butyl acrylate in (C) is 75% by mass or more. Resin composition. [Selection figure] None |