http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014025188-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1374dd16777534b65ad4422333245af8 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M15-693 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M13-395 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M15-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J161-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M15-41 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D02G3-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D02G3-40 |
filingDate | 2013-06-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0beaa61a45687c383deb48d6200e6be7 |
publicationDate | 2014-02-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2014025188-A |
titleOfInvention | Reinforcing fiber cord and manufacturing method thereof |
abstract | The present invention provides a reinforcing fiber cord and a method for producing the same, which have improved fraying properties and are excellent in adhesion to a matrix and fatigue properties (durability). The inner portion of the A fiber cord comprises a compound B 1 having a molecular weight of Compound A 1 of less than 1000, and less than Compound A 1 amounts, Compound Compound A 1 comprises an aromatic compound or an α- dicarboxylic acid component , and the compound B 1 is a compound a 1 other than the aliphatic compounds or alicyclic compounds, reinforcing fiber cord adhesive treatment agent is adhered to the surface. Furthermore, the adhesive treatment agent is a resorcin / formalin / latex (RFL) adhesive, the fiber cord is a twisted multifilament fiber, or is made of synthetic fiber, aromatic The group compound is preferably a heterocyclic compound. Moreover, and be unevenly distributed inner layer only in compounds A 1 of fiber cord, the presence of compounds containing hexamethylene diisocyanate (HDI) trimer structure fiber cords inner layer portion, there is a latex in the inner layer portion of the fiber cord Preferably not. The reinforcing fiber cord manufacturing method of the present invention is a manufacturing method of a reinforcing fiber cord in which the fiber cord is subjected to two-stage treatment with a pretreatment liquid and an adhesive treatment liquid, and the pretreatment liquid is a blocked isocyanate compound. A compound A 2 and a smaller amount of the blocked isocyanate compound B 2 , the block dissociation temperature of the compound A 2 is lower than the block dissociation temperature of the compound B 2 , and the fiber to which the pretreatment liquid is adhered In this manufacturing method, the cord is once heat-treated, and then an adhesion treatment liquid is attached and dried. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-3617397-A4 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2015092874-A1 |
priorityDate | 2012-06-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 69.