Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b9a255559e1d94f20510a17a673b1078 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-1133 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-1139 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-1131 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-1136 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-113 |
filingDate |
2012-07-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_50747e116fc9af41f958632a2505ca57 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f82cf4cdc58ecf56939c3c7abde029e7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_47b74db8ac3fe2dc78a5d4502d0b8bd0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_715f50351ade1c062207e07f07dca1f8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8263f27eb68f07a25ccf9cab108f6f5a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_82235234a723f4bf86bf3b3e3e9f23bd http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2982f82714e399da9a6f90f8c764cc93 |
publicationDate |
2014-02-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2014021360-A |
titleOfInvention |
Electrostatic latent image developer carrier and electrostatic latent image developer |
abstract |
To provide a carrier and a two-component developer capable of developing a stable toner amount without being affected by the toner consumption history of the immediately preceding image and obtaining a uniform image excellent in color reproducibility over a long period of time. . The carrier for an electrostatic latent image developer is obtained by coating the surface of a core material with a coating layer made of a resin containing conductive fine particles, and the conductive fine particle content in the coating layer is 58 wt. % To 73 wt%, the resistivity of the coating layer is 6.6 to 8.6 Ωcm, and in the FE-SEM reflected electron image on the carrier surface, the area ratio of the high-brightness contrast portion to the total particle area is 1% The electrostatic latent image developer carrier is less than (at an acceleration voltage of 0.8 KV) and 40% to 90% (at an acceleration voltage of 2.0 KV). [Selection figure] None |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015166809-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020052065-A |
priorityDate |
2012-07-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |