http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014009269-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6bfdf49224a405be1f7b653c56ebad94 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-642 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F10-02 |
filingDate | 2012-06-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_90683d41d54db21a07b83c1f1684e246 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b935795f4d12cfcacf3f41c17ef4fe29 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_86020d7c9b18ac9698674c35eb1d06d0 |
publicationDate | 2014-01-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2014009269-A |
titleOfInvention | Ethylene polymer |
abstract | PROBLEM TO BE SOLVED: To provide an ultra-high molecular weight ethylene polymer having sufficient wear resistance when used for fibers produced by gel spinning, etc. SOLUTION: Intrinsic viscosity ([η]) is 9.0 dL / g More than 20 dL / g, Mw is 1 million or more and 6 million or less, Mw / Mn is 3.0 or more and less than 4.0, and the proportion of the component having molecular weight (M) of less than 10,000 is 0.01% or less [M Is a calibration curve obtained from the values obtained by converting the molecular weight (peak top) of polystyrene (molecular weight distribution Mw / Mn <1.2) into the molecular weight of polyethylene using Q-factor and their elution times. In the above, an ethylene-based polymer having the same elution time component as the elution time of the corresponding molecular weight is shown. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016088946-A |
priorityDate | 2012-06-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 110.