Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9e1bf06f55de84b78abc9a057807f7eb |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D193-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D191-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L45-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L93-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D167-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D167-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-183 |
filingDate |
2012-06-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_98466a57880cfcd621620374508180c0 |
publicationDate |
2014-01-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2014005397-A |
titleOfInvention |
Aqueous dispersion and paint binder composition using the same |
abstract |
The present invention provides an aqueous dispersion that is excellent in water resistance and adhesion, and exhibits excellent coating performance with suppressed occurrence of cracks. A polyester resin (A) having an acid value of 3 mgKOH / g or more and a number average molecular weight of 5000 to 50000 and a tackifier (B) are represented by (A) / (B) = 95 / 5-30 / An aqueous dispersion characterized by containing in the range of 70 (mass ratio). Further, the polyester resin (A) preferably has a glass transition temperature of 30 ° C. or lower, crystallinity, and a melting point of 100 ° C. or lower. [Selection figure] None |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2015147145-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106133022-A |
priorityDate |
2012-06-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |