Predicate |
Object |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2989 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y40-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2002-82 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-64 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2006-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10S977-896 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G49-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G49-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G49-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y30-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07C51-412 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07F15-025 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07F15-02 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B82Y25-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C45-77 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C31-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C49-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C57-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B82Y5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B82Y30-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B82Y40-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C29-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C49-92 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C51-41 |
filingDate |
2011-06-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate |
2013-09-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2013536160-A |
titleOfInvention |
Synthesis and use of iron oleic acid |
abstract |
The present invention relates to a method of forming an iron oleic acid complex, the method comprising the following steps: (a) dissolving oleate in a lower alcohol solvent at a temperature of about 35 ° C. to 65 ° C .; (b) said step (A) adding a nonpolar solvent to the solution of (a); (c) adding an iron salt dissolved in a lower alcohol to the solution of FIG. (B); (d) heating the solution of step (c) to a temperature of about 50 ° C. (E) cooling the reaction mixture of step (d) to about 15 ° C. to 30 ° C .; (f) optionally filtering the reaction mixture of step (e); (g ) Separating the nonpolar solvent phase from the lower alcohol phase; (h) washing and drying the nonpolar solvent phase; (i) volatilizing from the nonpolar solvent phase in step (h) Comprises obtaining a and (j) Step (i) the individual iron oleate complex was mixed with a polar solvent of the product; step is removed by evaporation things. The present invention further provides an iron oleate complex obtainable by the process of the present invention, an iron oleate complex of the formula I, the use of the process iron oleate complex as a precursor for the production of nanoparticles, and an iron oxide / The present invention relates to a method for forming iron oxide nanoparticles comprising a suspension of hydroxide and the iron oleate complex of the present invention. |