http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013528686-A
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F212-08 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F212-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L9-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F236-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F4-48 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F236-10 |
filingDate | 2011-06-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2013-07-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2013528686-A |
titleOfInvention | Low vinyl content styrene-butadiene polymer and process for producing the same |
abstract | The present invention relates to an initiator and formula 1 wherein R1 and R2 are each independently C1-C4 alkyl, and R3, R4, R5, R6, R7 and R8 are each independently hydrogen or Polymerizing the monomer in the presence of at least one polar agent selected from C1-C4 alkyl), 1,2-diene is added to the polymerization and 1,2- Containing monomer units derived from styrene and 1,3-butadiene, the diene having a molar ratio of 0.1 to 1.0 and a molar ratio of polar agent to active initiator of 0.05 to 0.6 A method for continuous polymerization of polymers is provided. The present invention comprises A) a vinyl content of 12 to 40% by weight based on the weight of polymerized butadiene, B) a block styrene content of less than 8% by weight based on styrene weight and C) a styrene content of 10 to 50% by weight based on polymer weight Compositions comprising the polymer having are also provided. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10934382-B2 |
priorityDate | 2010-06-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |