Predicate |
Object |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T29-43 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-13 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G9-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G9-004 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G11-28 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G9-04 |
filingDate |
2010-07-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate |
2013-01-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2013501359-A |
titleOfInvention |
Solid electrolytic capacitor with improved ESR stability |
abstract |
An improved capacitor and a method of making a capacitor are described. The capacitor has an anode and a dielectric on the anode. A cathode layer is on the dielectric, wherein the cathode layer includes at least one conductive layer and an insulating adhesion enhancing layer. [Selection] Figure 2 |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014154466-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013239698-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2020218319-A1 |
priorityDate |
2009-07-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |