http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013239378-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_669c01133740c5233f2c8738904ea3af |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-48 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M2-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-131 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-134 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0566 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-052 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-1391 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-1395 |
filingDate | 2012-05-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b855f86c3b0cc6bdc02655a4aa7b64c1 |
publicationDate | 2013-11-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2013239378-A |
titleOfInvention | Non-aqueous electrolyte secondary battery electrode plate, non-aqueous electrolyte secondary battery, battery pack, and non-aqueous electrolyte secondary battery electrode plate manufacturing method |
abstract | [PROBLEMS] To prevent deterioration in cycle characteristics even when a material that has excellent output characteristics and expands in volume when alkali metal ions are inserted is used as a material for an electrode active material. An electrode plate for a non-aqueous electrolyte secondary battery, a non-aqueous electrolyte secondary battery and a battery pack using the same, and a method for producing a non-aqueous electrolyte secondary battery electrode plate having the above effects about. An electrode plate for a non-aqueous electrolyte secondary battery comprising a current collector and an electrode active material layer formed on at least a part of the surface of the current collector, wherein the electrode active material layer is an electrode. Active material particles and a binding material are contained, the electrode active material particles and the current collector, and the electrode active material particles are fixed together by the binding material, and the binding material is a polymer The half-width of the peak appearing at 980 to 1100 cm −1 of the Si—O bond obtained when the infrared absorption spectrum of the electrode active material layer is measured is 30 to 230 cm −1 . [Selection] Figure 1 |