http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013230660-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_73ebc284a55d5daf0e209d6186c9e65c |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41J2-01 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41M5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D11-00 |
filingDate | 2012-05-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4e98290740827f94acacee95951765ac http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2b0258a5eec8c4618f71701edf0e6d8c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2f2b231ceda45b666b81d6d7c82afe20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d080953dfef2f73d176b5e554807100a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ce9d2b9d0458924d7648a569944e2495 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c26acde3f0fcf40130c7fbe5bb76fcea |
publicationDate | 2013-11-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2013230660-A |
titleOfInvention | Manufacturing method of recorded matter and recorded matter |
abstract | The present invention provides a recorded matter that includes a printing portion that is observed through a base material, the printing portion is provided in a desired shape, and has an excellent gloss feeling like a mirror surface. A first ink application step for applying a first ink 2 'containing a first polymerizable compound 21' to a substrate 1, and a first curing step for polymerizing the first polymerizable compound 21 '. A second ink application step of applying a second ink 3 ′ containing the second polymerizable compound 32 ′ and the metal powder 31 onto the cured product 21 of the first polymerizable compound 21 ′, a second polymerization A second curing step for polymerizing the active compound 32 '. The contact angle of the first ink 2 ′ with respect to the substrate 1 is not less than 30 ° and not more than 85 °, and the droplets of the first ink 2 ′ land on the substrate 1, and the curing treatment for the droplets in the first curing step Within a second, the second ink 3 ′ droplets land on the cured product of the first polymerizable compound 21 ′ and the droplets are cured in the second curing step. Is 10 seconds or more. [Selection] Figure 1 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7048542-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020199650-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017036273-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016190959-A |
priorityDate | 2012-05-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 617.