Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e2b60c751b9b6855cd19a5127595779f |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-025 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F10-02 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29B11-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F10-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-6592 |
filingDate |
2013-03-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9e331de37f73c5a679af5bc626162d7e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f21fd87f139154672febca2c26e421ec http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2cc9b21f3bc0ec62318766159ce07fc2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3f941d6bb7e35d64af8646ab9f7031f6 |
publicationDate |
2013-11-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2013227539-A |
titleOfInvention |
Ethylene polymer for production of wear-resistant resin molded body, ethylene-based resin composition for production of wear-resistant resin molded body, wear-resistant resin molded body and method for producing the same |
abstract |
Disclosed is an ethylene polymer for producing a wear-resistant resin molded article having excellent wear resistance measured by a sand / rubber wheel wear test and having a good balance between moldability and heat resistance. [MEANS FOR SOLVING PROBLEMS] An ethylene-based polymer for producing an abrasion-resistant resin molded article that satisfies the following (1) to (5). (1) Ethylene homopolymer or copolymer of ethylene and an α-olefin having 3 to 20 carbon atoms (2) Polymerized using a single site catalyst (3) Weight average molecular weight Mw of 300,000 to 100 Less than 10,000 (4) Melting point Tm is 130 ° C. or more and less than 135 ° C. (5) Sand / rubber wheel wear performance measured on a test piece made from the ethylene polymer is 0.035 cm 3 or more and 0.24 cm 3 or less. ] None |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10738140-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019099804-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015140386-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102304973-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015174941-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015174942-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20190062922-A |
priorityDate |
2012-03-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |