http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013223954-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c1755eede76ea7e719a3e0d2843cd793 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7733c0176290f1fe4631514d71aee65e |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K105-06 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B27N3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/E04C2-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C43-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C43-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B27K5-00 |
filingDate | 2012-04-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2d2c638358617214336ba0e9e99a6ca6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_61c5317f4cb712999812608f4b937473 |
publicationDate | 2013-10-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2013223954-A |
titleOfInvention | Manufacturing method of wood-based composite material and wood-based composite material |
abstract | [PROBLEMS] To provide a method for producing a wood-based composite material that has a reduced swell coefficient due to water absorption, has good dimensional stability, and is capable of obtaining a light-weight and high-strength wood-based composite material, and the wood-based composite material A wood-based composite material manufactured by the manufacturing method is provided. [MEANS FOR SOLVING PROBLEMS] A chemical treatment step for obtaining a drug-treated strand by impregnating a wood strand with a low molecular weight phenolic substance that is cured and resinized by heating, and a binder adhesion for adhering a binder to the drug-treated strand. A laminated mat forming step of forming a laminated mat by laminating the treatment target strands to which the binder is adhered, substantially aligned in the length direction, and forming a laminated mat; and hot pressing forming the laminated mat A wood strand having a thickness of 0.1 to 1.0 mm, a fiber direction length of 20 mm or more, and an average length / thickness. The wood strands having a length of 100 to 500, an average length / width of 5 to 30, and a fiber length within the range of the average length ± 20% occupy 70% or more of the total wood strands. , And the said at mounting mat forming step, a target drug treatment strands with attached the binding agent, the production method of the wood composite material to be oriented at an angle of less than an average 24 ° to the longitudinal direction. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103770168-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-114589774-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-114589774-A |
priorityDate | 2012-04-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links