http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013216823-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_063a1b324005ddc15e16e7529c6258c4 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-02 |
filingDate | 2012-04-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5d44af937472716cee0e0cf28753c97b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_674fa19d6b0335d238d3876125ff90fb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ac30060266170485b28f31926f98043c |
publicationDate | 2013-10-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2013216823-A |
titleOfInvention | Manufacturing method of molding material, molding material, and fiber-reinforced resin molded body |
abstract | PROBLEM TO BE SOLVED: To provide a molding material manufacturing method, a molding material, and a fiber reinforced resin molded body capable of making a molded fiber reinforced resin molded body high in strength and uniform and suppressing occurrence of a scissors. A method for producing a molding material 6 comprising an unsaturated polyester resin and a reinforcing fiber, comprising coating a compound 20 comprising at least a thickener and an unsaturated polyester resin on the surface of a long reinforcing fiber, The compound 20 on the surface of the scale reinforcing fiber is thickened, and then the long reinforcing fiber covered with the compound 20 is cut into a predetermined length. [Selection] Figure 1 |
priorityDate | 2012-04-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |