http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013214075-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f83f063473c4431ded56a99529022290 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C45-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G09F3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G09F3-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D25-20 |
filingDate | 2013-05-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_527127e0cdcf5c95d326183e59014103 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b74c9ef855998f6d01db5d050e833e96 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_77fa0b9541c96ba24a5fbd09112e6027 |
publicationDate | 2013-10-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2013214075-A |
titleOfInvention | In-mold molding label and injection-molded body with the label |
abstract | [PROBLEMS] To provide an injection molded article made of a thermoplastic resin such as polyethylene terephthalate or styrene-acrylonitrile resin, which is not only a nonpolar resin but also a polar resin, and is excellent in water resistance, detergent resistance, chemical resistance and durability. Also provided are an in-mold molding label having excellent adhesive strength, and a labeled injection-molded body to which the in-mold molded body label is attached. The present invention comprises a laminated resin film including a base layer and a porous adhesive layer, the surface area ratio of the porous adhesive layer is 6 to 30%, and the porous adhesive layer is under a pressure near atmospheric pressure. In-mold molding label that has been subjected to plasma treatment, and when the label is applied to an injection molded body made of an ester resin or a styrene resin to form a labeled injection molded body, the molded label and the injection Adhesive strength with the molded body is 200 to 800 gf / 15 mm, and the adhesive strength between the label and the injection molded body after dipping the labeled injection molded body in a surfactant solution for 24 hours is 150 to 600 gf / 15 mm. A label for in-mold molding. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-5701461-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7338151-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2018062128-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015166175-A |
priorityDate | 2013-05-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 45.