http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013199519-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_129e393582e6bdf4029baf2206522f45 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L77-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-04 |
filingDate | 2012-03-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0f0a425bffb1422c8a518790784ce3e7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b26473fbe711fd62ba798741c2d18656 |
publicationDate | 2013-10-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2013199519-A |
titleOfInvention | Thermoplastic resin composition and molded article thereof |
abstract | 【Task】 To provide a thermoplastic resin composition having an excellent balance between mechanical properties and antistatic properties. [Solution] The rubber polymer (r) is composed of an aromatic vinyl monomer (a1), a vinyl cyanide monomer (a2), and other vinyl monomers (a3) copolymerizable therewith. Graft copolymer (A) 20 to 40 parts by weight, polyamide elastomer (B) 5 to 15 parts by weight, polyamide resin (C) 40 to 70 parts by weight. And 5 to 20 parts by weight of a modified vinyl copolymer (D) having at least one functional group selected from the group consisting of a carboxyl group, an epoxy group, an amino group and an amide group in the molecular chain. (However, the total content of the components (A) to (D) is 100 parts by weight), a thermoplastic resin composition. [Selection figure] None |