http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013189626-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_24aca9ded2638ea793d05360dde7a4a0 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2666-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2312-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T156-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-14 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F299-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-0869 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C45-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C45-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C45-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-24 |
filingDate | 2013-01-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1a52275173b29a919095cf1cfa45db07 |
publicationDate | 2013-09-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2013189626-A |
titleOfInvention | Method for producing thermoplastic elastomer composition and method for producing composite molded body |
abstract | Disclosed is a composite molded body in which a molded body made of a thermoplastic elastomer composition and a molded body made of a polyamide resin are fused with sufficient strength without providing an adhesive layer. And a method for producing a thermoplastic elastomer composition capable of providing such a composite molded body. A method for producing a thermoplastic elastomer composition comprising kneading 100 parts by weight of a thermoplastic elastomer and 15 to 120 parts by weight of an ethylene copolymer containing (C) an unsaturated carboxylic acid unit, The thermoplastic elastomer is obtained by dynamically vulcanizing (A) 50-90% by weight of an oil-extended ethylene-α-olefin copolymer rubber and (B) 10-50% by weight of a propylene resin in the presence of a crosslinking agent. (The total amount of component (A) and component (B) is 100% by weight), The (A) oil-extended ethylene-α-olefin copolymer rubber is composed of 100 parts by weight of an ethylene-α-olefin copolymer rubber having a Mooney viscosity (ML 1 + 4 100 ° C.) at 100 ° C. of 150 to 350 and mineral oil. The said manufacturing method containing 20-150 weight part of type | system | group softeners. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020172626-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7235724-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020532604-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2022071498-A1 |
priorityDate | 2012-02-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 161.