Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9b6b5f6c667accdd7bc86416835388aa |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-13 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G11-74 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M50-571 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M50-543 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M50-531 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M50-116 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M50-124 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0525 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G11-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M50-571 |
filingDate |
2012-03-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6132cd0395ba39f62481ca117150a8fb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a821720ec0a02473a6c9c99fc0a71edc http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a96604d3436ad8780706fee0f2bb49dc |
publicationDate |
2013-09-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2013187018-A |
titleOfInvention |
Electrode lead wire member for non-aqueous battery |
abstract |
Even if the electrolyte of a lithium ion battery reacts with moisture to generate hydrofluoric acid and increase its corrosiveness, the corrosion resistance is improved so that the adverse effect is avoided and the life of the lithium ion battery is extended. An electrode lead member for an aqueous battery is provided. An electrode lead wire member is drawn from a non-aqueous battery storage container using a laminate film laminate of an aluminum foil and a resin film as an exterior material. A protective layer 22 is formed on the surface by applying and drying a solution containing a polyvinyl alcohol resin or polyvinyl ether resin and a fluorine compound. The fluorine compound is water-soluble, and the protective layer 22 is formed on the outer surface of the metal flat plate 21 in a belt-like pattern by printing. [Selection] Figure 4 |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-5760138-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017134962-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016081792-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015156365-A |
priorityDate |
2012-03-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |