http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013141794-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_33dafb5bbc2ec47ebcb7becbbe60f704 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K19-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K23-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K105-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K59-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K29-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L29-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C45-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L53-02 |
filingDate | 2012-01-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8d9cbb299f0ce9d9a9de9d80df3c391d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a52b97aa2c0f6b18e19e4cfcaf4edb97 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2ec410a9361c5d10a11899996d8d6047 |
publicationDate | 2013-07-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2013141794-A |
titleOfInvention | Manufacturing method of adhesive body |
abstract | An object of the present invention is to provide a method for producing an adhesive body by insert molding, which can firmly join an insert part and a thermoplastic polymer composition even in a relatively low temperature of 30 to 150 ° C. of the insert part. A method of manufacturing an adhesive by insert molding in which a mold holding an insert part is filled with a thermoplastic polymer composition and molded, the polymer block containing an aromatic vinyl compound unit; , 2-bond amount and 3,4-bond amount in combination with a block copolymer having an isoprene unit, a butadiene unit or a polymer block containing an isoprene / butadiene unit, or a hydrogenated product thereof A thermoplastic polymer composition containing 1 to 100 parts by mass of a polyvinyl acetal resin (B) and 5 to 100 parts by mass of a polar group-containing polypropylene resin (C) with respect to 100 parts by mass of a certain thermoplastic elastomer (A). The manufacturing method of an adhesive body which uses and the temperature of the insert components at the time of insert molding shall be 30-150 degreeC. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2021181999-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017095617-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109504023-A |
priorityDate | 2012-01-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 181.