Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_268be9afa00cf55b5aa72b1612151ecb |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-31986 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K2323-035 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L1-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B23-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K19-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-3025 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-17 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L1-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02F1-1335 |
filingDate |
2012-11-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9a2173e21a18260794cc797874ef1841 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e6fab274c55efcee093080d26d382a37 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b16536ff91b17aab9450099a7819ba54 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_14f13ce7b68c83ff39709757cee4f06e |
publicationDate |
2013-06-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2013127058-A |
titleOfInvention |
Cellulose acylate film, polarizing plate protective film, polarizing plate and liquid crystal display device |
abstract |
Disclosed is a cellulose acylate film having excellent scratch resistance and capable of maintaining sufficient adhesion to an active energy ray cured layer such as a hard coat layer even when irradiated with light for a long period of time. A minimum value of Knoop hardness measured by rotating a Knoop indenter at the same indentation position with a indentation load of 50 mN according to the method of JIS Z 2251 is 170 N / mm 2 or more and 220 N / mm 2 or less. A cellulose acylate film containing 0.001 mass% or more and 5 mass% or less of a cellulose compound with respect to cellulose acylate. [Selection figure] None |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20160121415-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20170131652-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2015378073-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10338290-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2015151683-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9453952-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2016111316-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015214707-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2015151683-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2016178371-A1 |
priorityDate |
2011-11-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |