http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013116954-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_24aca9ded2638ea793d05360dde7a4a0 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L69-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-12 |
filingDate | 2011-12-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3f288fc92418a8c9eb5f4c972574771f |
publicationDate | 2013-06-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2013116954-A |
titleOfInvention | Resin composition, method for producing the same, and molded article |
abstract | To provide a resin composition excellent in both transparency and heat resistance in a mixed resin of a polycarbonate resin and an acrylic resin. The resin composition of the present invention comprises (a) an acrylic resin, (b) a polycarbonate resin, and (c) a copolymer of an unsaturated nitrile monomer and an aromatic vinyl monomer. Include in specific proportions. Furthermore, the method for producing a resin composition according to the present invention comprises (a) an acrylic resin, (b) a polycarbonate resin, and (c) a copolymer of an unsaturated nitrile monomer and an aromatic vinyl monomer. Is melt-kneaded at a shear rate of 10 to 5000 sec −1 at a temperature of 150 to 350 ° C. [Selection figure] None |