Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_24aca9ded2638ea793d05360dde7a4a0 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F6-84 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-60 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-605 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01D1-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01D5-08 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-19 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-84 |
filingDate |
2011-11-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_24ac2f7211fb8529fb91c203fc7e1871 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2f8169fa88353997d70b46f1648b7474 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0b37a8e9af3d67283200186ba4ba1ef9 |
publicationDate |
2013-06-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2013108191-A |
titleOfInvention |
Textile manufacturing materials and fibers |
abstract |
An object of the present invention is to provide a fiber manufacturing material capable of improving fiber strength. A fiber manufacturing material comprising a liquid crystal polyester that satisfies the following requirements (a) and (b). (A) The weight average molecular weight is 30000 or less, and the polydispersity is 2.5 or less. (B) Using a flow characteristic tester, the melt viscosity measured at 360 ° C. under a nozzle hole diameter of 0.5 mm and a shear rate of 1000 s −1 is 70 Pa · s or less. [Selection figure] None |