Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a8a9982b1666c54b5bf02d6c944891e4 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C3-095 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03B17-064 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03B17-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C3-087 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C3-091 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C3-095 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03B17-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C3-091 |
filingDate |
2013-02-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ff485fe31d0a381a858fb434b1814325 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_31f71ccd3c81449d6709bfa41df68fa2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0301faa183bb2510e3d0399d4bcaba39 |
publicationDate |
2013-05-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2013082626-A |
titleOfInvention |
Glass composition having high thermal and chemical stability and method for producing the same |
abstract |
Kind Code: A1 An alkali-free glass exhibiting desired physical and chemical properties for a liquid crystal display substrate. In mole percent on an oxide basis, SiO 2 64.0-72.0 Al 2 O 3 9.0-16.0 B 2 O 3 1.0-5.0 MgO + La 2 O 3 1.0-7.5 CaO 2.0-7.5 SrO 0.0-4.5 BaO 1.0-7.0 Including Here, the BaO / SrO ratio in mole percent is 2.0 or more, It has a strain point of 700 ° C or higher. [Selection figure] None |